Electrodissolution aluminum electrode during an electrocoagulation acid whey

dc.contributor.authorReyes Cruz, Victor Esteban
dc.date.accessioned2016-05-23T21:33:30Z
dc.date.available2016-05-23T21:33:30Z
dc.date.issued2014
dc.description.abstractElectrodissolution of aluminum in solutions containing chloride or sulfate ions during electrocoagulation acid whey, has been the objective of this work. The alkaline pH increases the rate of dissolution by several orders of magnitude. The electrolytic medium (Cl- or SO42-) does not seem to significantly influence the dissolution of aluminum, but increase the charge density, which helps in the electrochemical process. The results are related to the nature of aluminum hydroxide species formed during anodic dissolution. In acidic and neutral conditions, OH-ions from the cathode do not fully participate in the formation of neutral species of aluminum hydroxide and excess OH-ions increases the pH of the medium. In contrast, the pH decreases in highly alkaline conditions attributed to the consumption of large amounts of OH- ions to form an anionic species such as Al(OH)4- and Al(OH)52-, and other polymeric species of aluminun.es
dc.identifier.citationPrieto García Francisco, Callejas-Hernández Judith, Reyes-Cruz Víctor Esteban, Marmolejo-Santillán Yolanda, Prieto Méndez Judith (2014), "Electrodissolution aluminum electrode during an electrocoagulation acid whey",DYNA 81 (187), pp. 129-136es
dc.identifier.urihttps://repository.uaeh.edu.mx/bitstream/123456789/16900
dc.languagees
dc.subjectRecubrimientos y Corrosiónes
dc.titleElectrodissolution aluminum electrode during an electrocoagulation acid wheyes
dc.typeArticle

Archivos

Bloque original

Mostrando 1 - 1 de 1
Cargando...
Miniatura
Nombre:
dyna_electrodisolucion.pdf
Tamaño:
456.41 KB
Formato:
Adobe Portable Document Format

Colecciones